Probe Software Users Forum

Software => CalcImage => Topic started by: John Donovan on January 26, 2019, 01:21:49 PM

Title: Variation/Correlation Plotting In CalcImage
Post by: John Donovan on January 26, 2019, 01:21:49 PM
We implemented a variation/correlation plotting method for quantitative pixel calculations in CalcImage from the Polygon/Pixel Filtering Extraction window as seen here:

(https://smf.probesoftware.com/gallery/1_26_01_19_12_38_59.png)

This variation plot method works for the shape extraction, polygon extraction and also line profile extraction methods. Here is an example using a 10 x 10 pixel shape extraction:

(https://smf.probesoftware.com/gallery/1_26_01_19_12_39_24.png)

Again, as with the variation plotting in Probe for EPMA, if you click on one of the graphs, the plot is expanded as seen here:

(https://smf.probesoftware.com/gallery/1_26_01_19_2_44_40.png)

If you decide to plot the quant pixels for the whole x-ray map image, be aware that as the number of pixels gets larger than 100K or so, the plotting slows down, but it does display eventually:

(https://smf.probesoftware.com/gallery/1_26_01_19_12_49_36.png)

and again one can display a single element pair correlation:

(https://smf.probesoftware.com/gallery/1_26_01_19_12_49_48.png)