Hi,
Suddenly I cannot save the spectra in SVG. Now, there are only options to save them in bitmap format (TIFF, JPEG, PNG, BMP). No possibility to save the spectrum in the vector graphic (Debian Buster 5.10.0-0.bpo.5-amd64, DTSAII, Microscopium 2021-01-06 revision). The same on the old box running Win7 and the identical version of DTSAII.

Please, could you send me some hints or advice?

I am thanking you in advance.

Oldrich
Title: Re: SVG export in DTSA-II Microscopium
Post by: jrminter on July 08, 2021, 06:08:24 AM
You might try the latest prerelease version here:

https://drive.google.com/file/d/17YAXRYkQ9vAQ509AwP5eZagdGfShX-dE/view?usp=sharing

It is dated 2021-05-03
Title: Re: SVG export in DTSAII Microscopium
Post by: Nicholas Ritchie on July 09, 2021, 08:01:59 AM
I don't remember exactly when I removed SVG support from DTSA-II.  It was a few years ago before I move to Github and lost my previous change record.   
I'm sorry if you found it useful but it was getting hard to continue to support.

Nicholas
Title: Re: SVG export in DTSAII Microscopium
Post by: Oldrich on July 21, 2021, 12:09:55 AM
Thank you all for your replies. I am sorry for the late reply. I was out of the institute.

Best regards