When calibrating your imported image file in PictureSnap, it's usually easier to first select two diagonally oriented features to get the picture calibrated for translation and scale.
After you have calibrated the picture for two points, simply select a 3rd calibration point roughly on the corner of a triangle including the two original calibration points, and drive to the approximate stage position of this third calibration point by double-clicking the picture.
Then select the "Three Points" calibration option (the image will now be listed as "Image Is Uncalibrated") and after manual X/Y stage adjustment of the third point feature, read the stage coordinates and select the picture coordinates.
Then click the Calibrate Picture button and the picture will now be calibrated for image rotation.
To further calibrate the imported PictureSnap image for Z stage tilt, simply use the Move To buttons for each calibration point to drive to that stage position, adjust the stage Z, then click the Read Current Stage Coordinate button. After all three points have been confirmed for Z focus, just click the Calibrate Picture button *again* and your picture is now calibrated for Z stage tilt in addition to image rotation.
John,
I often use my flatbed scanner to scan an image of the complete sample shuttle (either 4x thin sections or 6x 25mm rounds). I then use reference marks marked on my shuttle to calibrate the image; these are very fast to locate (because +/_ a few um, they are always in the same place!) and allow me to calibrate multiple sample locations all at once. Only problem with this is the z calibration is not in the plane of the sample surface. For this reason, it might be useful if the Z coordinate was also displayed, so it could be manually edited??
gareth
John
Would it be feasible to allow multiple PictureSnap windows to run simultaneously? This would be very useful for using overview and detailed images concomitantly. I know it is possible to run Stage! and PictureSnap together to achieve the same thing, but setting-up PictureSnap is more efficient.
Gareth
Quote from: Gseward on July 17, 2013, 12:42:56 PM
I often use my flatbed scanner to scan an image of the complete sample shuttle (either 4x thin sections or 6x 25mm rounds). I then use reference marks marked on my shuttle to calibrate the image; these are very fast to locate (because +/_ a few um, they are always in the same place!) and allow me to calibrate multiple sample locations all at once. Only problem with this is the z calibration is not in the plane of the sample surface. For this reason, it might be useful if the Z coordinate was also displayed, so it could be manually edited??
Good idea. I can do that but you'll have to remember to click the Calibrate Image button if you edit them manually.
Quote from: Gseward on July 17, 2013, 01:59:52 PM
Would it be feasible to allow multiple PictureSnap windows to run simultaneously? This would be very useful for using overview and detailed images concomitantly. I know it is possible to run Stage! and PictureSnap together to achieve the same thing, but setting-up PictureSnap is more efficient.
PictureSnap is designed to allow a resizable full view and 1:1 pixel mapping at the same time. So if your scan is very high resolution, you can see the whole thing using the
Full Image Picture View menu and then see the detail using the regular PictureSnap window.
So here is a cool example of importing a CL image from our Quanta SEM and importing it into PFE's PictureSnap feature while the sample was loaded in the EPMA.
There was considerable sample rotation, ~10 degrees from the student not being especially careful, but first the two point calibration was performed, then the third point was added to correct for rotation and the PFE analysis positions line up exactly where they were digitized in the EPMA for both the probe BSE and the SEM CL images.
Here's another tip for PictureSnap:
To display your currently digitized coordinates (position samples listed in the Automate! window), use the Display menu from the PictureSnap window.
To display your currently acquired coordinates (std, unk or wav samples listed in the Analyze! window), use the Run menu from the main PFE window. This also works in data reprocessing mode when not connected to the instrument.
This is mainly a tip for Cameca users, but in any event you've all probably noticed that the default installation of Probe for EPMA and CalcImage assumes a JEOL stage orientation. This is simply because most EPMA instruments "out there" are JEOL instruments!
For Cameca users, that means when you install PFE for off-line data and image re-processing you will be loading Cameca oriented images into an "assumed" JEOL stage orientation. What will this look like? Well, your Cameca micron stage units will be converted to mm as seen here, and another thing: the image is "flipped"!:
(https://smf.probesoftware.com/oldpics/i40.tinypic.com/vxhfef.jpg)
Obviously something is wrong! Yes, in converting from Cameca to JEOL coordinates systems, not only did the units change from um to mm, but the stage orientation changed from Cameca Cartesian orientation to JEOL "anti-cartesian" orientation!
To see your stage units in microns again, and the image properly oriented, as seen here:
(https://smf.probesoftware.com/oldpics/i43.tinypic.com/n53mnr.jpg)
you'll need to copy some Probe for EPMA config files over from your on-line instrument computer to the off-line re-processing computer as described in this post which is linked here (note this only has to be done once for each off-line re-processing computer or whenever you update your standard composition database, Standard.mdb):
https://smf.probesoftware.com/index.php?topic=76.msg280#msg280
Actually for the purposes of this post, a Cameca user really only needs to copy over the following files, but it doesn't hurt to make a back up of the other files:
Probewin.ini
motors.dat
scalers.dat
crystals.dat
standard.mdb
Here's a cute trick for digitizing points at low mag in PFE (use the Confirm Positions options in the Automate! window later to get the z focus exact!), using either an imported low mag SEM image, flat bed scanner image or even an analog (SE, BSE) image acquired and then exported from PFE.
The SEM or flat bed scanner image will need to be calibrated using the instructions here:
https://smf.probesoftware.com/index.php?topic=14.msg28#msg28
though the exported PFE image will already have a calibration, so it's even easier. Simply export a low mag image using the Save As BMP button as seen here:
(https://smf.probesoftware.com/oldpics/i42.tinypic.com/54ns8.jpg)
and then import into PictureSnap as seen here:
(https://smf.probesoftware.com/oldpics/i40.tinypic.com/2vc6kxl.jpg)
and then you can use this menu to digitize points for acquisition using this menu:
(https://smf.probesoftware.com/oldpics/i43.tinypic.com/22dkja.jpg)
Finally, use the Display menu in PictureSnap to see the points as you digitize them and then using the right mouse, click on the approximate positions desired for acquisition on the PictureSnap image:
(https://smf.probesoftware.com/oldpics/i44.tinypic.com/2q2hikm.jpg)
Be sure to confirm them for proper position and exact z stage focus from the Automate! window prior to acquisition!
John,
Maybe I have missed documentation somewhere. I am seeing two issues with Picturesnap when trying to load larger images.
All images we use are jpg images
1. If the image is "way too big" there is an out of memory error
2. If the image is large, then only a portion of the image is loaded into PS
It would be preferable to know in advance what the pixel limitations are if that is possible, or to have PFE tell me that an image is too large for loading and will be clipped.
I am seeing the clipping of the image for images that are, for example, 3000x4000 or so. We previously limited images to 2kx2k but you told me very large images can be loaded, so we tried.
I don't view the clipping as a feature, and I am pretty sure all users would prefer to have the image loaded in entirety or have a message explaining why it could not be loaded.
The other issue is that I have users who show up with jpg images but they are 24 bit deep. Is there a limitation on bit depth with jpgs?
Cheers,
Paul
After off-line discussion with Donovan I now see issues that likely will affect users:
1. It is video memory that is used for Picturesnap images. If your PC has only basic video graphics or an older card (our PFE computer has an ATI FireGL v7200 which has "only" 256 mb of video ram) then I suppose it is possible to run out of memory with a large PS image. We are running two monitors at 2560x1600 and 1920x1080 all the time.
2. Is is possible to calculate the size of the image one is trying to load and open a dialog when the image is clipped for the normal window and also to avoid the out of memory error with an informative dialog that shows the size of the image trying to load and the available video memory (is is possible to determine the amount of video memory available).
Users tend to come to the lab with very large scanned images or mosaics that have not been downsampled but the sheer size is usually apparent from inspection. It seems like having a video card with 1 gb or more video memory would be a good upgrade for users.
Paul
Edit by John: Unfortunately the Microsoft call only returns "OK" or the error number, no other information. Did you try opening the Full View window from the PictureSnap menu? Your best bet is to get a video card with more memory as you stated above, but I've also been able to load bigger images by reducing the video card display mode to 16 bit color depth. See comments in attached FAQ.
A question, John:
I use Picture Snap on my online PC and I display "currently acquired coordinates" and it works just fine. I took the file and went to my offline PC, and there the displayed points do not line up with the image any more. They are shifted. Why is that? Are there any ini files that might be different? Is it not just comparing the jpg calibration coordinates with the analyzed positions coordinates?
Quote from: Philipp Poeml on April 18, 2016, 07:56:24 AM
A question, John:
I use Picture Snap on my online PC and I display "currently acquired coordinates" and it works just fine. I took the file and went to my offline PC, and there the displayed points do not line up with the image any more. They are shifted. Why is that? Are there any ini files that might be different? Is it not just comparing the jpg calibration coordinates with the analyzed positions coordinates?
Hi Philipp,
Yes, it should work.
I've tested this issue some time ago on different monitors and it seemed to work, but maybe the monitors you used have different DPI values? I'm not sure what could cause this honestly. I've sort of standardized on 24" monitors in my lab which makes this issue hard to test. I know the PictureSnap calibration works for sure if the monitors are the same. I will look into it again though just to double check.
You can try exporting the config files on your off-line computer from the File | Export Configuration menu in PFE, but all necessary values should already be stored in the MDB file.
Hm... Then it could be the dpi. The dpi is definitely different in the lab and in the office. There is no way around to have the points displayed correctly on different screens?
Quote from: Philipp Poeml on April 19, 2016, 03:36:37 AM
Hm... Then it could be the dpi. The dpi is definitely different in the lab and in the office. There is no way around to have the points displayed correctly on different screens?
Hi Philipp,
As I said above, I think getting the same size monitor on both computers, might be a "way around". I can't offer a better solution until I understand the problem and for that I need more observations on when it works and when it doesn't and by how much. For example, is it just a difference in monitor size that causes this offset, or is it a difference in monitor DPI? Or is it caused by a different aspect ratio? I do not know yet...
Let's work together off-line on this and see if we can figure out exactly what what is causing the offset. Then I can fix it.
Edit by John: It was a DPI difference in the monitors and this issue is now handled automatically in PictureSnap.
Quote from: Philipp Poeml on April 18, 2016, 07:56:24 AM
A question, John:
I use Picture Snap on my online PC and I display "currently acquired coordinates" and it works just fine. I took the file and went to my offline PC, and there the displayed points do not line up with the image any more. They are shifted. Why is that? Are there any ini files that might be different? Is it not just comparing the jpg calibration coordinates with the analyzed positions coordinates?
I had the same issue with my laptop monitor (Sony VAIO). When I go to see the picture snap with points of analysis I notice they are all shifted with respect to their original position. The computer is running under Windows 7. Screen's resolution is 1366x768 (recommended). I clicked "make text or other items larger or smaller" in screen resolution window and selected "Medium 125%" (see attachment). That resolved the issue.
Quote from: Philipp Poeml on April 19, 2016, 03:36:37 AM
Hm... Then it could be the dpi. The dpi is definitely different in the lab and in the office. There is no way around to have the points displayed correctly on different screens?
Good news. I finally found a solution for the PictureSnap screen DPI issue when displaying stage coordinates on an image, that was acquired on a monitor with a different screen resolution. It is now fixed.
Basically this is the Windows screen resolution parameter when, under Win 7, you right click the desktop, select the Screen Resolution menu, select the Make Text and other items larger or smaller link, and select one of the options. Usually one will see 100% (the default), 125% and 150%.
(https://smf.probesoftware.com/gallery/1_03_12_17_5_25_14.png)
The new PictureSnap code saves this screen resolution DPI to the .ACQ file (along with the other calibration parameters) when the image is saved. When the image (in PictureSnap) is displayed on another monitor, the new code adjusts the screen calibration so the image and the stage coordinates are properly displayed.
This code will work on all ACQ files generated since 6/29/2017 (v. 11.9.4). If you have an older ACQ file, simply re-generate the ACQ file by exporting it again, or by re-running the calibration on the original computer/monitor. The ACQ file will be updated properly with v. 12.1.0 or higher of PFE.
Alternatively one can simply edit the old ACQ file for the new parameter as seen here:
[stage]
PictureSnap mode="0"
Number of calibration points="2"
Number of Z calibration points="0"
Screen reference point1 (twips)="7680,7680"
Screen reference point2 (twips)="0,0"
Stage reference point1="50.2185,50.6295"
Stage reference point2="50.4815,50.3705"
X_Polarity="-1"
Y_Polarity="-1"
Stage_Units=mm
ACQScreenDPI="1"
Where the ACQScreenDPI is the DPI of the monitor that the image was acquired on, and 1 = 100%, 1.25 = 125% and 1.5 = 150%. So just edit the ACQ file in any text editor for the DPI of the system it was acquired on and save the file. It should then load fine in PictureSnap on any DPI monitor now.
Odd that this different DPI monitor issue only showed up in PictureSnap, not any other places where stage coordinates are plotted on images. And sorry it took me so long to find a solution, it was actually pretty simple once I understood the problem. Thanks.
john
PS Attached below are images with a stage coordinates plotted, for both 1.0 and 1.25 screen DPI.
I had forgotten that there was a PictureSnap Tips and Tricks topic already!
I wanted to ask if anyone has tried the new PictureSnap from the PFE Digitize Traverse or Digitize Grid dialogs, where there is now a PictureSnap button in each dialog that allows one to see a line (for digitizing traverses) or a rectangle (for digitizing grids) on the PictureSnap image. Here is what it looks like for a traverse:
https://smf.probesoftware.com/index.php?topic=42.msg6529#msg6529
and here is what is looks like for a grid:
https://smf.probesoftware.com/index.php?topic=42.msg6527#msg6527
Has any one tried this feature yet? What do you think?
Hi John
I desperately want to, but haven't had a working probe for over a month now so cant try out all the new cool features that were implemented last year. It looks like a cool feature which looks like it will definitely save a lot of time. I especially like the main PictureSnap window adjusting to where you move to. Once its all up and running I will have a play with it and let you know what the users think of it.
Cheers
Here is a new feature in PictureSnap suggested by Ben Vos.
(https://smf.probesoftware.com/gallery/1_25_04_18_6_41_56.png)
Basically the software will now display the image extents of any images acquired and saved in the currently open PFE probe database. To use the feature acquire some images in PFE and save them to the database. Then load an image into the PictureSnap window that includes the area the images are located in. Normally this will be a "basemap" image which could be a camera image of the sample, a slide scanner image or even a low mag image. Then click the Display | Display Acquired Image FOVs menu as seen here:
(https://smf.probesoftware.com/gallery/1_25_04_18_6_42_13.png)
The images areas and the image number will be displayed in both the main PictureSnap image window and the full view window as seen here:
(https://smf.probesoftware.com/gallery/1_25_04_18_6_42_30.png)
Let me know what you think after you all have tried it out. Thanks!
The image calibration accuracy display in PictureSnapApp is so useful that we added it to Probe for EPMA also:
(https://smf.probesoftware.com/gallery/1_21_06_18_12_54_23.png)
Paul Carpenter suggested adding a feature to PictureSnap in Probe for EPMA that allows one to select an already existing ACQ file for calibrating a new image.
(https://smf.probesoftware.com/gallery/1_26_06_18_3_19_21.png)
The idea being that some labs take a picture of a sample with almost the same area and mounted in the same location in the sample holder.
This way one can have some "generic" ACQ files available for getting a rough image calibration loaded and then tuning it a bit using the Move To buttons.
The latest version of Probe for EPMA now correctly displays the current FOV graphic, if your sample is loaded into the instrument at an angle to the scanned image. Here is the FOV graphics (blue rectangle), once we subsequently rotated the image after it was in the instrument:
(https://smf.probesoftware.com/gallery/1_01_07_18_2_07_55.png)
Now here is the new "rotation sensitive" current FOV graphic on the original (unrotated) scanned image:
(https://smf.probesoftware.com/gallery/1_01_07_18_2_08_38.png)
This rotated FOV graphic indicates that the image coordinate system is rotated with respect to the stage coordinate system. Note that PictureSnap handles such rotated samples just fine for sample navigation, but previously it wasn't reflecting the image to sample rotation correctly in the current FOV graphic.
We'll be doing the same thing for PictureSnapApp but it will be a bit more work given that the FOV annotations and Image Locator feature can require rotated objects as well...
Owen Neill was recently running PictureSnapApp on his JEOL SEM (more on this later) and really likes the option to disable the Z axis for stage motion when navigating the sample. This is for when using a three point image calibration (so the image is also calibrated in Z), and the Z axis sample heights vary a lot.
He suggested that I add the same option to the PictureSnap feature in Probe for EPMA. So here it is:
(https://smf.probesoftware.com/gallery/1_15_09_18_5_15_16.png)
Update PFE from the Help menu.
Hi,
Is there a way to display only analysis locations from one unknown position list on an image in PictureSnap, rather than all locations from all position lists?
My user carefully chose a series of well-placed points on her specimen. Later that day, I inadvertently ran a grid of many points over the same location, making it impossible to read her original locations when the image is opened in PictureSnap. If we could just load "her" points, and ignore my grid, we could see exactly which grains she hit...
Thanks!
Em
Quote from: emma_fisi on November 19, 2018, 11:21:24 AM
Hi,
Is there a way to display only analysis locations from one unknown position list on an image in PictureSnap, rather than all locations from all position lists?
My user carefully chose a series of well-placed points on her specimen. Later that day, I inadvertently ran a grid of many points over the same location, making it impossible to read her original locations when the image is opened in PictureSnap. If we could just load "her" points, and ignore my grid, we could see exactly which grains she hit...
Thanks!
Em
Hi Emma,
If you are referring to displaying previously acquires analysis positions on the PictureSnap image (from the Run menu) in Probe for EPMA, then an easy way would be to check the "Skip Disabled Points On PictureSnap" menu, and then simply disable the samples you do not displayed from the Analyze! window. Once you are done you can enable them again from the Analyze! window.
john
Thanks John! I'll give this a try on the morrow.
Hello all,
We are trying to import a photo of our stage in the Picture Snap option within the Stage software, but our photo is showing up a) rotated, and b) way too big to be of use, unless we go into the menu and click view full picture.
We then rotated and compressed our picture, and re-imported it, but it's still displaying sideways. Is it a directionality with our camera that's affecting the meta data?
Seems like a silly problem, but I'm just wondering if I missed something in the reference manuals...
Thanks
Odd. Does the image show properly in other image apps?
If the image is very large just use the scroll bars to navigate. Please email me the image, and we'll take a look, but also show me a thumbnail showing how you think it should be oriented.
john
Hi All! John, this Picture Snap app (text input) is working great moving between our Tescan and SIMS instruments!
The issue for us is that we can't see our sample material, unlike those wonderfully colorful and swirly geologic samples. The picture we take of our sample basically looks like a blank planchet, so adding annotations by clicking on a point of interest on the sample picture is a no-go. Is there a way to add to the annotation list manually by typing in x and y coordinates instead of going through the Picture Snap image?
Quote from: bgarcia on July 15, 2020, 04:25:47 PM
Hi All! John, this Picture Snap app (text input) is working great moving between our Tescan and SIMS instruments!
The issue for us is that we can't see our sample material, unlike those wonderfully colorful and swirly geologic samples. The picture we take of our sample basically looks like a blank planchet, so adding annotations by clicking on a point of interest on the sample picture is a no-go. Is there a way to add to the annotation list manually by typing in x and y coordinates instead of going through the Picture Snap image?
Hi Ben,
Glad that you find it useful!
You can add a position annotation to the current position by typing "<shift> p" as described in the PSA "quick start" document from the Help menu:
To annotate points on the image, simply right-click the image and enter a text string.
To annotate the current FOV on the image, type "<shift> f" on your keyboard and enter a text string. To annotate the current position on the image, type "<shift> p" on your keyboard and enter a text string.
Ok, I got the [shift P] to work, but our issue is that we can only annotate a comment and can't change the x-y coordinates themselves using the list of annotated points.
Even though we are at some x-y coordinate on our instrument, we don't really know where that is on the image without clicking over and over on the image to have the exact matching x-y numbers pop up in the annotate box. There are no lines or shapes (or anything, really) to be able to find where we are on the PicSnap image (of our sample). I was hoping there was a direct text input way to add both a point and annotation without having to click or otherwise interact with the PicSnap image. That way, we could save a list of points using our instrument stage coordinates without ever having to find them first on the PicSnap image. Once the points are saved, then they would of course appear on the image. Does that make sense?
Hi Ben,
Having a calibrated image is the whole point of PictureSnapApp! :)
If the sample surface doesn't have any identifying features that you can find, can you utilize the edges of the sample, or perhaps make some calibration marks on the sample such as the fiducial marks we make on our standard mounts?
https://smf.probesoftware.com/index.php?topic=172.msg8991#msg8991
john
:-[ ;)
I just found the missing piece: I didn't notice the x-y counter in the title bar of the window. :o That solves everything! ugh
Explaining my problem helped, so.. yay?
Yeah!
So are you running PictureSnapApp in "text input" mode on your microprobe? You have to use "text input" mode on the SIMS, but on your EPMA instrument you can connect to the instrument to automatically read the mag and stage positions.
john
No, these samples are being used between SIMS and a Tescan SEM. ;D
Ah.
Yes, "text input" is what you'll have to use on those instruments as we only support JEOL and Cameca microprobes, JEOL 7000 SEMs and FEI instruments directly.
https://probesoftware.com/PictureSnapApp.html
john
Ive been using PicSnap a bit more, and a workflow issue has come up. Keep in mind, I'm using the text input version on a Tescan SEM for use in a Cameca SIMS.
What we hope to do, facilitated by PicSnap, is find small (1-10 micron) particulate in the Tescan and save a list of 10-20 locations using the annotation list feature. Then send that image/acq file to the SIMS so that THEY can find the same particles. The trouble I've had is that in order to find a location on the Tescan and annotate that place in PicSnap, I have to move the mouse cursor over the PicSnap image to the exact x/y coordinates shown on the Tescan. I really thought this would be easier.. it sounds easy. It is do-able, but extremely time-consuming and not really accurate. The PicSnap image x/y space isn't up/down to move in the x direction and left/right to move in the y direction because there's usually some rotation it is accounting for. This makes moving the mouse cursor in an exact fashion really hard and frustrating. For the text input version, it's easy to transfer location from PicSnap to another instrument, but difficult to go from another instrument into PicSnap.
Is there an easy way to implement something like an X-Y-Z coordinate display like an instrument with a stage might have? It would display the coordinates of the bullseye in PicSnap, and allow for one to type in some location and have the PicSnap bullseye "move" to that location, like a virtual stage. It would make finding a Tescan location in PicSnap so much easier, and allow me to then accurately save that location in the annotation list quickly and accurately.
Hi Ben,
So in the "connected" version of PictureSnapApp for JEOL/Cameca/FEI instruments the app is always reading the current stage position and the "bullseye" always indicates that current position.
What you are asking for, is for the free "text input" version (which doesn't actually communicate with the instrument), to have a way to indicate the current stage position?
So perhaps I should just add a "Move" button to the PictureSnapApp Display Current Position dialog (using a double-click with the mouse) and you can simply enter the current coordinates from the Tescan instrument and the "bullseye" will move to that position? For subsequent annotation...
Yes, that's it! Exactly. Otherwise there's no direct way to get actual stage coordinates over to PicSnap. ;D ;D
Another helpful button/menu-option would be "annotate stage position" or "add stage position to annotated positions".
Hi Ben,
OK, I think I've got what you want:
(https://smf.probesoftware.com/gallery/1_13_08_20_1_39_40.png)
So in text input mode when you double-click it pops up the "current stage position" dialog as before, but there's a new button that allows you to enter any position on your instrument, and then move the current position cursor to that position on the image. Then you just click "<shift> "p" and you can annotate the position (or <shift> "f" for a FOV annotation).
However, in *any* instrument mode you can also click on the Window menu and click the new "Current Stage Position" menu and this same window will now pop up and you can do similar operations.
Just use the Help menu to update PictureSnapApp to v. 1.7.9 and let me know what you think.
No surprise here, but it works! Nice job! This is exactly what we needed. You have some happy clients at PNNL. :D
This is a very small change in the PictureSnap feature in Probe for EPMA, but Gareth Seward requested it and we finally got around to implementing it.
So in the main PictureSnap window there is a menu that one can check to enable the digitizing of analysis positions in the Automate! window as seen here:
(https://smf.probesoftware.com/gallery/1_04_07_22_12_04_00.png)
Previously this feature only digitized points that were right clicked on from the main PictureSnap window, but Gareth wondered if we could add support for this right click digitize feature also from the "full view" image window. That is now implemented in the latest version of Probe for EPMA as seen here:
(https://smf.probesoftware.com/gallery/1_04_07_22_12_04_16.png)
Of course, as usual, one can subsequently confirm these digitized points from the Automate! window to ensure that the optical Z focus (and X/Y positions) are exactly correct.
We've improved the display of digitized and acquired points on the PictureSnap window in the latest version of Probe for EPMA (v. 13.6.6). Here is the slightly modified PictureSnap Display menu for displaying digitized position samples from the Automate! window:
(https://smf.probesoftware.com/gallery/1_05_11_23_8_47_20.png)
The only thing we changed was to improve some error trapping (no samples displayed or selected in the Automate! window) and re-arrange the menus slightly. Here is what is looks like when the points are displayed:
(https://smf.probesoftware.com/gallery/1_05_11_23_8_47_44.png)
But for displaying already acquired sample positions from the Analyze! window we've added a feature that was only available for digitized points which is to display only the points for a single selected sample in the Analyze! window:
(https://smf.probesoftware.com/gallery/1_05_11_23_8_48_01.png)
Quote from: John Donovan on November 05, 2023, 08:56:49 AM
But for displaying already acquired sample positions from the Analyze! window we've added a feature that was only available for digitized points which is to display only the points for a single selected sample in the Analyze! window:
(https://smf.probesoftware.com/gallery/1_05_11_23_8_48_01.png)
This is nice. Any chance it could be made to work for multiple selected samples? For when an analytical session involves several sample changes and several picture changes? I currently disable the other points. Although alternatively for each sample change I would have to make a new file. (It would be also good to have ability refresh/reload content for when display options already checked, maybe in form of button or when image loaded?)
What I do also like and only found recently is the disable z option and allow picture snap to only move in x and y -which is great where samples different heights - a very nice feature
Quote from: Ben Buse on September 19, 2024, 06:45:17 AMQuote from: John Donovan on November 05, 2023, 08:56:49 AMBut for displaying already acquired sample positions from the Analyze! window we've added a feature that was only available for digitized points which is to display only the points for a single selected sample in the Analyze! window:
(https://smf.probesoftware.com/gallery/1_05_11_23_8_48_01.png)
This is nice. Any chance it could be made to work for multiple selected samples? For when an analytical session involves several sample changes and several picture changes? I currently disable the other points. Although alternatively for each sample change I would have to make a new file. (It would be also good to have ability refresh/reload content for when display options already checked, maybe in form of button or when image loaded?)
What I do also like and only found recently is the disable z option and allow picture snap to only move in x and y -which is great where samples different heights - a very nice feature
These are good ideas.
After a bit of work, we were able to modify the selected sample option from the Run menu to allow selection of a single or multiple samples in the Analyze! sample list to be displayed on the PictureSnap image:
(https://smf.probesoftware.com/gallery/1_20_09_24_2_35_09.png)
In fact it's such a good idea that we did the same for the display of digitized points from the Automate! window:
(https://smf.probesoftware.com/gallery/1_20_09_24_2_36_59.png)
In addition we modified the click events in both the Analyze! sample list and the Automate! position list to update the display in PictureSnap automatically.
8)
Update as usual from the Help | Update Probe for EPMA menu...
Just downloaded the update, and enjoying
This is great
Based on suggestions from Gareth Seward in addition to the Home key press feature:
https://smf.probesoftware.com/index.php?topic=1020.msg13389#msg13389
we've added another new feature to the PictureSnap (and PictureSnapApp) full view window which is that a right double click using the mouse on the full view image window, will move the main image to that location without moving the stage.
The only complication is in Probe for EPMA when the Use Right Mouse Click To Digitize Positions menu is checked in the PictureSnap window. If this menu is checked then a right mouse click or double-click digitizes a point in the Automate! window instead. However, I added code to ignore the right click (click or double-click) if the Automate! window is not visible But if the menu is not checked it works fine as expected and just moves the main image to that location.