Post by: wrigke on September 02, 2026, 12:16:48 PM
Does anyone have any experience with Periodic Today standards?
https://www.periodictoday.com/

Are they good quality?

Thanks!
Karen
Title: Re: Periodic Today standards
Post by: Probeman on September 08, 2026, 01:28:54 PM
Quote from: wrigke on September 02, 2026, 12:16:48 PMDoes anyone have any experience with Periodic Today standards?
https://www.periodictoday.com/

Are they good quality?

You might ask Will Nachlas if he's dealt with them. 
Title: Re: Periodic Today standards
Post by: Sander on September 30, 2026, 02:34:02 AM
Quote from: wrigke on September 02, 2026, 12:16:48 PMDoes anyone have any experience with Periodic Today standards?
https://www.periodictoday.com/

Are they good quality?

Thanks!
Karen

Happy customer here.  Highly reccommended.