Currently our PFE log window displays wt% with three digits after the decimal point. For trace element measurement, we would like to see ppm level concentrations. How to display elemental or oxide wt% with 4 or 5 digits after the decimal point in the log window? Thanks.
Quote from: Donggao Zhao on April 03, 2015, 02:15:21 PM
Currently our PFE log window displays wt% with three digits after the decimal point. For trace element measurement, we would like to see ppm level concentrations. How to display elemental or oxide wt% with 4 or 5 digits after the decimal point in the log window? Thanks.
Hi Donggao,
Good question!
From the Analytical | Analysis Options dialog, simply check the Use Automatic Format For Quantitative Results checkbox as seen here:
(https://smf.probesoftware.com/oldpics/i57.tinypic.com/34gvs7q.jpg)
You'll have two choices, both are useful for trace element analyses.
The first is what you asked for, it gives the maximum number digits possible. The second, formats based on sensitivity and detection limit. So a normal output looks like this:
ELEM: P P P P P Zr Si O SUM
XRAY: (ka) (ka) (ka) (ka) (ka) (la) () ()
179 -.012 .002 .000 .004 .025 50.088 15.323 34.913 100.342
180 .003 .001 .001 -.019 .000 49.584 15.323 34.913 99.806
181 .005 .004 -.001 .002 -.021 49.794 15.323 34.913 100.019
182 -.006 -.001 -.008 -.001 .001 49.676 15.323 34.913 99.897
183 .009 -.006 .008 .014 -.005 49.718 15.323 34.913 99.975
AVER: .000 .000 .000 .000 .000 49.772 15.323 34.913 100.008
SDEV: .009 .004 .006 .012 .016 .192 .000 .000 .203
SERR: .004 .002 .003 .005 .007 .086 .000 .000
%RSD: ---- ---- ---- ---- ---- .39 .00 .00
PUBL: n.a. n.a. n.a. n.a. n.a. 49.764 15.323 34.913 100.000
%VAR: --- --- --- --- --- (.02) .00 .00
DIFF: --- --- --- --- --- (.01) .000 .000
STDS: 285 285 285 285 285 257 0 0
And the first option outputs like this:
ELEM: P P P P P Zr Si O SUM
XRAY: (ka) (ka) (ka) (ka) (ka) (la) () ()
179 -.01235 .00239 -.00034 .00366 .02467 50.0875 15.3230 34.9130 100.342
180 .00322 .00124 .00133 -.01930 .00027 49.5837 15.3230 34.9130 99.8065
181 .00521 .00356 -.00112 .00231 -.02082 49.7941 15.3230 34.9130 100.019
182 -.00556 -.00143 -.00805 -.00107 .00123 49.6762 15.3230 34.9130 99.8974
183 .00946 -.00576 .00821 .01434 -.00540 49.7178 15.3230 34.9130 99.9746
AVER: .00000 .00000 .00001 -.00001 -.00001 49.7719 15.323 34.913 100.008
SDEV: .00881 .00371 .00581 .01223 .01638 .19210 .000 .000 .20333
SERR: .00394 .00166 .00260 .00547 .00732 .08591 .00000 .00000
%RSD: ---- ---- ---- ---- ---- .38596 .00000 .00000
PUBL: n.a. n.a. n.a. n.a. n.a. 49.7640 15.3230 34.9130 100.000
%VAR: --- --- --- --- --- (.02) .00 .00
DIFF: --- --- --- --- --- (.01) .00000 .00000
STDS: 285 285 285 285 285 257 0 0
The second option output looks like this:
ELEM: P P P P P Zr Si O SUM
XRAY: (ka) (ka) (ka) (ka) (ka) (la) () ()
179 n.d. n.d. n.d. n.d. .02 50.1 15.323 34.913 100.3
180 n.d. n.d. n.d. n.d. n.d. 49.6 15.323 34.913 99.8
181 n.d. n.d. n.d. n.d. n.d. 49.8 15.323 34.913 100.0
182 n.d. n.d. n.d. n.d. n.d. 49.7 15.323 34.913 99.9
183 .009 n.d. .008 .01 n.d. 49.7 15.323 34.913 100.0
AVER: n.d. n.d. n.d. n.d. n.d. 49.8 15.323 34.913 100.01
SDEV: .009 .004 .006 .012 .016 .192 .000 .000 .203
SERR: .004 .002 .003 .005 .007 .086 .000 .000
%RSD: ---- ---- ---- ---- ---- .386 .000 .000
PUBL: n.a. n.a. n.a. n.a. n.a. 49.764 15.323 34.913 100.000
%VAR: --- --- --- --- --- (.02) .00 .00
DIFF: --- --- --- --- --- (.01) .000 .000
STDS: 285 285 285 285 285 257 0 0
Hope that helps!
john