Hi,
I'm hoping someone can help. How do you get "Calculate Projected detection limits" to work I've checked it & "calc detection limits & sensitivity" but I can't see the projections in the log window. Any ideas what I doing wrong I'm sure I'm missing something - I remember we had this on a ancient version of Probe for Windows. I ask because I havn't time to enter the information into my excel spreadsheet to calculate it
Thanks
Ben
Quote from: Ben Buse on May 03, 2016, 07:37:59 AM
I'm hoping someone can help. How do you get "Calculate Projected detection limits" to work I've checked it & "calc detection limits & sensitivity" but I can't see the projections in the log window. Any ideas what I doing wrong I'm sure I'm missing something - I remember we had this on a ancient version of Probe for Windows. I ask because I havn't time to enter the information into my excel spreadsheet to calculate it
Hi Ben,
Odd, it works for me (see below).
I think you have to have at least two or three data points?
john
Detection Limit (t-test) in Elemental Weight Percent (Average of Sample):
ELEM: Th Hf U P Y
60ci .001 .001 .001 .000 .001
80ci .001 .001 .001 .000 .002
90ci .002 .002 .002 .000 .003
95ci .003 .002 .002 .001 .004
99ci .004 .003 .004 .001 .006
Predicted Detection Limits (99% CI) in Elemental Weight Percent (Average of Sample):
ELEM: Th Hf U P Y
TIME: 640.00 640.00 640.00 640.00 640.00
BEAM: 100.54 100.54 100.54 100.54 100.54
PRED: .008 .006 .004 .001 .005
Projected Detection Limits (99% CI) in Elemental Weight Percent (Average of Sample):
ELEM: Th Hf U P Y
TIME: 10.00 10.00 10.00 10.00 10.00
PROJ: .035 .028 .031 .007 .047
TIME: 20.00 20.00 20.00 20.00 20.00
PROJ: .025 .020 .022 .005 .034
TIME: 40.00 40.00 40.00 40.00 40.00
PROJ: .018 .014 .015 .003 .024
TIME: 80.00 80.00 80.00 80.00 80.00
PROJ: .012 .010 .011 .002 .017
TIME: 160.00 160.00 160.00 160.00 160.00
PROJ: .009 .007 .008 .002 .012
TIME: 320.00 320.00 320.00 320.00 320.00
PROJ: .006 .005 .005 .001 .008
TIME: 640.00 640.00 640.00 640.00 640.00
PROJ: .004 .003 .004 .001 .006
TIME: 1280.00 1280.00 1280.00 1280.00 1280.00
PROJ: .003 .002 .003 .001 .004
TIME: 2560.00 2560.00 2560.00 2560.00 2560.00
PROJ: .002 .002 .002 .000 .003
TIME: 5120.00 5120.00 5120.00 5120.00 5120.00
PROJ: .002 .001 .001 .000 .002
TIME: 10240.0010240.0010240.0010240.0010240.00
PROJ: .001 .001 .001 .000 .001
TIME: 20480.0020480.0020480.0020480.0020480.00
PROJ: .001 .001 .001 .000 .001
TIME: 40960.0040960.0040960.0040960.0040960.00
PROJ: .001 .000 .000 .000 .001
Analytical Sensitivity (t-test) in Elemental Weight Percent (Average of Sample):
ELEM: Th Hf U P Y
60ci .000 .000 .000 --- ---
80ci .000 .000 .000 --- ---
90ci .000 .000 .000 --- ---
95ci .000 .000 .000 --- ---
99ci .000 .000 .000 --- ---
Thanks John yes I was trying it for a single point when I do it for 3 points it works :)
Ben