News:

:) Welcome to the Probe Software forum area!

Main Menu

GunAlign (8900/8200/8500 only)

Started by John Donovan, July 03, 2014, 04:29:28 PM

Previous topic - Next topic

John Donovan

The GunAlign app has recently been improved with assistance from Owen Neill (WSU) and Anette von der Handt (UMN).

Note the new buttons for reading and setting the HV status:



Note that the scroll bars don't always operate as expected. One issue is that the JEOL instrument rounds off some parameters, so for example if you are at 3700x and click the scroll arrow to increment mag by 10 (to 3710), the instrument returns 3700 still...

However, the text entry followed by <enter> will usually work fine.
John J. Donovan, Pres. 
(541) 343-3400