Philipp Poeml

BTW, any suggestions for the other ideas?

In addition: Our standard ring is quite large. I would like to save some time driving around, so I would like to change the order the standards are measured in. How would I do that?

Cheers
Ph

John Donovan

Quote from: Philipp Poeml on November 03, 2015, 05:46:11 AM
In addition: Our standard ring is quite large. I would like to save some time driving around, so I would like to change the order the standards are measured in. How would I do that?

Cheers
Ph

Yeah, I've been thinking about a good idea to do this.

Not an ideal method, but since PFE runs standards in numerical order, if you number your standards in the order they should be run...