News:

:) To see the latest forum posts scroll to the bottom of the main page and click on the View the most recent posts on the forum link

Main Menu

No more rainbows!

Started by Anette von der Handt, December 21, 2017, 03:29:09 PM

Previous topic - Next topic

Probeman

Quote from: SteveSeddio on February 21, 2023, 01:54:40 PM
I happened to be perusing some Optometry journals (as one does), and the only color ramp that I saw was rainbow!
The irony!

What about bee optometry journals?   They see in the ultraviolet!    :D
The only stupid question is the one not asked!

Probeman

What's worse than a rainbow palette?

This:

The only stupid question is the one not asked!

anenburg

This is an excellent paper on the topic, for those who are interested.

https://doi.org/10.1038/s41467-020-19160-7

Anette von der Handt

That is a great paper! Thanks for sharing.
Against the dark, a tall white fountain played.

Anette von der Handt

Hi,

I created color scales (Viridis, Cividis, Magma and Plasma) for the JEOL N-Map viewer. See here for the files and instructions how to implement it: https://smf.probesoftware.com/index.php?topic=1529.0

Against the dark, a tall white fountain played.

JonF

Here's the link for the viridis, cividis, plasma and magma colour scales for use with CalcImage:

https://smf.probesoftware.com/index.php?topic=1615.msg12579#msg12579

John Donovan

This fall has quite colorful, enough so that I can almost see a "full spectrum" from our house:

John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"