Quantitative Trace Element X-ray Mapping

Started by Probeman, November 07, 2013, 04:15:30 PM

Previous topic - Next topic

Probeman

Here's an example of a set of quantitative x-ray maps we did earlier this year of a hydrothermal quartz sample, showing trace level variation (though no detectable Ti) and the pixel level detection limits:



The only stupid question is the one not asked!

Probeman

#1
Another example at the same conditions as above. First the quant weight percents:



And here the quant detection limits:

The only stupid question is the one not asked!

Probeman

#2
It is interesting to compare the above weight percent image in the first post, in which the color scale was adjusted manually, seen here again:



With this image below, which are the same data but just displayed using the automatic log scaling with no adjustment. The only downside I can see to the log scaling is that you have to calculate the actual weight percents from the log values in one's head!



For more information on point analyses of trace elements in quartz, see this post:

http://smf.probesoftware.com/index.php?topic=29.msg387#msg387