News:

:) To protect your privacy, you must first log in before you can view forum statistics and user profiles

Main Menu

Standard Materials Available

Started by John Donovan, August 01, 2014, 02:46:19 PM

Previous topic - Next topic

John Donovan

All,
At the recent Cameca user's meeting (which included a few JEOL users as well!), we discussed some ideas regarding standards. Anette Von der Handt suggested that we start to organize the community to create a priority list of new standard materials that should be developed. Suggestions for new materials should be made to this topic:

http://smf.probesoftware.com/index.php?topic=301.0

In the meantime, I thought it might be useful to create a topic of standard materials that exist already and are available in sufficient quantities for distribution.

To start that process I would like to offer an ultra high purity Ti metal produced by growth in 1000 degrees iodine vapor.  This material has been characterized for O, N and C which is quite unusual. The oxygen is the largest contaminant at 80 PPM. The chunk I have is about 10 grams so I could divide it up into a number of pieces. I need to figure out how to cut it up, probably using a wire saw.

To avoid getting overwhelmed by requests for this fine material, I'd like to ask that each requester also reciprocate and post in this topic another standard material that they can provide to the community in exchange for receiving the ultra pure Ti.  So please make your request for this Ti metal in a post where you offer a standard material of your own that you have available for exchange or just for distribution if you don't need a standard material in exchange.

How does that sound?
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Ben Buse

Does anyone have any synethic foresrite to share Mg2SiO4, I see you mention it both in above post and above M&M poster.

I also see Peter McSwiggen presented on peak shifts in Mg system - using 2nd order line - so more visible
https://academic.oup.com/mam/article/32/Supplement_1/ozag053.836/8742788

John Donovan

Quote from: Ben Buse on August 11, 2026, 08:56:34 AMDoes anyone have any synethic foresrite to share Mg2SiO4, I see you mention it both in above post and above M&M poster.

I also see Peter McSwiggen presented on peak shifts in Mg system - using 2nd order line - so more visible
https://academic.oup.com/mam/article/32/Supplement_1/ozag053.836/8742788

Ben is referring to this post and attached poster presentation pdf:

https://smf.probesoftware.com/index.php?topic=1831.msg14457#msg14457

This synthetic Mg2SiO4 material is available from this company:

https://www.opt-oxide.com/en/
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"