Our SX100 "Visualisation" board is producing some "digital hash" on the display monitor, but not in the data itself.  Not a huge deal, but sometimes it makes it a little hard to navigate around.

We'd like to try another "Visualisation" board if any one has a spare they could lend us, just to see if that solves the problem.  The board part# on the schematic is:

CIE Visualisation
39245068/040-C

I suspect the last part is a revision number so might not be critical.  Does any one have a spare board we could try out to see if the problem persists?  We'd return if it of course, unless it solves the problem and someone is willing to sell it to us...
The only stupid question is the one not asked!

Philipp Poeml

John, we have a spare one, but it is far from you. I am not sure it makes sense to send it all the way from Europe. Anyway, let us know, we could try to figure something out...

Probeman

Quote from: Philipp Poeml on September 02, 2015, 11:59:55 PM
John, we have a spare one, but it is far from you. I am not sure it makes sense to send it all the way from Europe. Anyway, let us know, we could try to figure something out...
Cool!

Let me contact you off-line.