Yes, at low count rates and also because the Mg Ka and Al Ka PHA peaks are pretty narrow and can be adjusted to stay within the differential window (is that what you mean by "normal PHA settings"?).

The benefits for the integral baseline method show up more for emission lines with an escape peak:

https://smf.probesoftware.com/index.php?topic=1854.msg14601#msg14601

and also for very wide peaks like O Ka:

https://smf.probesoftware.com/index.php?topic=1854.msg14619#msg14619

If you have the K-411/412 NBS/NIST glasses try extrapolating from SiO2, MgO and Fe3O4 (or Fe2O3) to these mineral glasses... or the USGS BIR basaltic glasses are pretty accurate also.