Edwards 306A Coater Problems

Started by Ben Buse, July 14, 2026, 09:19:14 AM

Previous topic - Next topic

Ben Buse

Hi

Has anyone seen a 'A FRAME ERROR' on Edwards Auto 306?

Unfortunately I didn't take a picture, after Fine Pumping appeared.

Ben Buse

#1
Here's next question where should the blue wire in the attached photos be attached. I think it tells the system whether the diffusion pump has warmed up, and with it disconnected it assumes the diff pump has already warmed up

JonF

Quote from: Ben Buse on July 20, 2026, 02:17:08 AMHere's next question where should the blue wire in the attached photos be attached. I think it tells the system whether the diffusion pump has warmed up, and with it disconnected it assumes the diff pump has already warmed up

There are some really fantastically helpful images of the Edwards Auto 306 on the UniGreenScheme website, in particular this one:




This looks like the plug you're referring to, and seems to be missing from your images. I suppose the next question is why is it disconnected? Please make sure that unit is unplugged and properly powered down/discharged before you go inside the case!

NB it might be worth downloading all the images from that website locally.
Link here and another one here

The instruction and maintenance manuals for the turbo version of the 306 are also online at U.Arizona here and here



Ben Buse

#3
Well spotted, thanks, now how to attach it...

Ben Buse

#4
It's labelled in diff pump manual https://www.precisionplus.com/medias/1-Manual-Edwards-EO-EO2K-EO4K-EO6K.pdf?context=bWFzdGVyfHJvb3R8MTQ1MDAzMnxhcHBsaWNhdGlvbi9wZGZ8YURJMUwyZ3hOQzh4TmpNME5EWTFOVFUyTURjek5DOHhYMDFoYm5WaGJGOUZaSGRoY21SelgwVlBYMFZQTWt0ZlJVODBTMTlGVHpaTExuQmtaZ3xlMDhlZTdkN2QxZWZiNWQ4NmFkODI4NzRhNGY3YjI3ZmVkMjI4MGRiY2UxODhjMTBkMGNhZjBjYzNmNzdlZDU3&attachment=true as pump ready thermal snap switch B02304000. Part no longer available but not essential, without it, it just assumes diff pump already warmed up, because of how it's broke, so metal contact no longer being pushed down by the base.

Switches detailed here https://www.idealvac.com/files/brochures/edwards_diffusion_pumps.pdf

I'll be getting a alternative comparable thermal switch

Ben Buse

#5
Has anyone ever used Plasmaglo on Edwards 306? If so a helpful explanation of how to use it, would be great. We seem to have inherited one. That's assuming it is one, I thought it was a radiant heater, anyone know what it looks like

It's mentioned in manual https://cores.arizona.edu/sites/default/files/attachments-service/e090-02-860.pdf