film thickness monitor crystals

Started by Ben Buse, September 22, 2026, 01:42:47 AM

Previous topic - Next topic

Ben Buse

Hi

Do all coaters use the same film thickness monitor crystals? Where do people buy replacements from? Or how do they clean them?


Ben Buse

Ok this site suggests https://www.microtonano.com/EM-Tec-quartz-crystals-for-thickness-monitor-controllers-for-vacuum-coating-systems.php two types a 6Mhz and 5Mhz with different diameters with brands using different ones as shown in table

Probeman

Quote from: Ben Buse on September 22, 2026, 01:42:47 AMHi

Do all coaters use the same film thickness monitor crystals? Where do people buy replacements from? Or how do they clean them?

Maybe it's too "old school" but I've always had great success using the color on polished brass method for checking carbon evaporation thickness:

https://smf.probesoftware.com/index.php?topic=1252.msg8988#msg8988
The only stupid question is the one not asked!