Ben Buse

Hi,

Just found my script to quantify k-ratios, so I thought I'd post it before I lose it again

import dtsa2 as dtsa2
import dtsa2.mcSimulate3 as mc3


f = open('C:/Users/Ben/Documents/FeKR.csv', 'r')
FeLines = f.readlines()
print(FeLines)
f.close()
FeLines4 = [float(FeLines[0].strip()),]
for x in range (1,9):
FeLines4.append(float(FeLines[x].strip()));
print(FeLines4)
f = open('C:/Users/Ben/Documents/NiKR.csv', 'r')
NiLines = f.readlines()
f.close()
NiLines4 = [float(NiLines[0].strip()),]
for x in range (1,9):
NiLines4.append(float(NiLines[x].strip()));
print(NiLines4)
for x in range (0,9):
print quant(kratios = {transition('Fe K-L3'):FeLines4[x],transition('Ni K-L3'):NiLines4[x]})



The files are as below: txt files - list of k-ratios separated by return.

0.9
0.8
0.7
0.6
0.5
0.4
0.3
0.2
0.1

Philippe Pinard

Here is my modified version of DTSA2 with a special class (MassAbsorptionCoefficientCalculator) to calculate MACs from X-ray intensities measured at different kVs:
https://www.dropbox.com/s/bf3wx3n5f7rg2r4/epq.jar?dl=0

and in attachment, an example of a script, which we used for this paper Llovet, X.; Pinard, P. T.; Heikinheimo, E.; Louhenkilpi, S. & Richter, S. Electron Probe Microanalysis of Ni Silicides Using Ni-L X-Ray Lines Microscopy and Microanalysis, 2016, 1-11 and I used in my PhD thesis.

Note that you need to fit intensities, not k-ratios.

QuoteI don't know about DTSA-II, but what you describe is exactly what Pouchou's XMAC software does.

One difference with DTSA-II is that you can use different PRZ models and fit "unconventional lines" like Ll, etc. but I agree that XMAC also works well. The main reason I wrote a special class was to be able to fit the MAC of more than one X-ray line, e.g. Ni La and Fe La from a binary Fe-Ni sample.

Ben Buse

Hi Philippe,

Thanks that's great -yes i've read the paper and that's the kind of thing I want to do. Do you know which version of DTSA its compatible with - I replaced Iona epq but it no longer loads

Thanks

Ben

Probeman

Hi Ben,
I found that proceedings volume and scanned it, so the Pouchou paper you wanted is attached below (please login to see attachments).
john
The only stupid question is the one not asked!

Ben Buse

#4
Hi John,

Thanks for finding the right paper! and scanning it

Method is easy - take generated phi-rho-z curve and modify mac so absorbed phi-rho-z curve matches data. I've just done this in excel using solver and casino for the generated phi-rho-z curves. In sheet 1 - can calculated mac used in casino 2159 for Fe La in Fe - i.e. similar to MAC30 not FFAST.

In sheet 2 - took Pouchou 1985 data for Ni at 10,15,20,25,30kV. Solve it and get mac of 3368 similar to Pouchou value of 3300 for Ni La in Ni and a long way from book value due to white lines - (peak in absorption spectra).

Ben

Ben Buse

Hi,

Does anyone know Pouchou & Pichoir expression for ionisation cross section, - I found a reference to J. L. Pouchou, F. Pichoir, in: 11th ICXOM, London Ontario, 1986 (J. D. Brown, R. H. Packwood, eds.), London, Ont, 1987, p. 249. Does anyone have a copy

Thanks

Ben

Brian Joy

Hi Ben,

It's also contained in their 1991 paper in Electron Probe Quantitation.  I've attached a copy.

Brian
Brian Joy
Queen's University
Kingston, Ontario
JEOL JXA-8230

Ben Buse

Hi Brian,

Thanks, Oh good I've good the green book, I'd missed the section - found it now