Hi John,

today I did the following:
I set up a file with U at peak 58402. Backgrounds were +1000 and -1000.

Then I went to this window:

(https://smf.probesoftware.com/oldpics/i61.tinypic.com/2ij3ew8.jpg)

and I was looking at the peak and decided it should be at 58410 instead. So I right-clicked to update the on peak position.

I was surprised when I realized later, that my backgrounds were not +1000 and -1000 anymore, but they were -1008 and +992.

Can this be right?

Cheers
Philipp
Title: Re: Display peaks and choose new peak position
Post by: John Donovan on April 10, 2014, 09:57:29 AM
Quote from: Philipp Poeml on April 10, 2014, 05:23:48 AM
I was surprised when I realized later, that my backgrounds were not +1000 and -1000 anymore, but they were -1008 and +992.  Can this be right?

Well, I guess it depends on what someone wants, but I will make it consistent with the other dialogs and update the off-peaks also.
Title: Re: Display peaks and choose new peak position
Post by: Philipp Poeml on April 11, 2014, 01:08:10 AM
Thank you John. I think it is better like this. If the peak moves, the backgrounds should move as well.