Hi John,

today I did the following:
I set up a file with U at peak 58402. Backgrounds were +1000 and -1000.

Then I went to this window:



and I was looking at the peak and decided it should be at 58410 instead. So I right-clicked to update the on peak position.

I was surprised when I realized later, that my backgrounds were not +1000 and -1000 anymore, but they were -1008 and +992.

Can this be right?

Cheers
Philipp

John Donovan

Quote from: Philipp Poeml on April 10, 2014, 05:23:48 AM
I was surprised when I realized later, that my backgrounds were not +1000 and -1000 anymore, but they were -1008 and +992.  Can this be right?

Well, I guess it depends on what someone wants, but I will make it consistent with the other dialogs and update the off-peaks also.
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Philipp Poeml

Thank you John. I think it is better like this. If the peak moves, the backgrounds should move as well.