News:

:) All Electron Probe Micro-Analysts are welcome to register and post!

Main Menu

Stage increment for unknown and standard acquisition?

Started by JohnF, April 03, 2015, 06:17:02 PM

Previous topic - Next topic

JohnF

Working with FE probe means a much more intense beam, so there is (or should be) a certain amount of experimentation. Certainly TDI is one useful tool. Another useful tool would be the ability to jog the stage (or continuously move it) while counting either as a standard or an unknown (clearly on a homogeneous material). In PfE there is a clear ability to do this with wavescans. However, I do not see it for unknown or standard acquisitions. Is it there somewhere, where I just don't see it? Or it not there, it would be a useful addition to the PfE toolkit.

John Donovan

#1
Quote from: JohnF on April 03, 2015, 06:17:02 PM
Working with FE probe means a much more intense beam, so there is (or should be) a certain amount of experimentation. Certainly TDI is one useful tool. Another useful tool would be the ability to jog the stage (or continuously move it) while counting either as a standard or an unknown (clearly on a homogeneous material). In PfE there is a clear ability to do this with wavescans. However, I do not see it for unknown or standard acquisitions. Is it there somewhere, where I just don't see it? Or it not there, it would be a useful addition to the PfE toolkit.

Hi John,
Yes, the stage stepping option for wavescans as seen here:



...was designed for sulfur peak shift measurements for determining chemical oxidation state.  The problem is that if one leaves the beam too long on an alkali glass, the trace sulfur will begin to oxidize, compromising the peak shift characterization...

But I do understand your point, so try the Alternating on/off Peak method.  This tracks the net intensity over time.

And if the sample really is homogeneous, why not just defocus the beam?
john
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

JohnF

#2
This is not for direct quant analysis, so the issue of sample homo/heterogenity is not relevant.

This is  for "experimental tool kit" work... trying to understand some complex (charge build up?) behavior in the intense FE beam.

As it is, I have to manual move the stage when acquiring counts and absorbed beam current, to hit 'unzipped' areas every second or so...seems like PfE should have this option (even if vulcan power fist salut required).


Probeman

#3
Quote from: JohnF on April 06, 2015, 12:30:47 PM
This is not for direct quant analysis, so the issue of sample homo/heterogenity is not relevant.

This is  for "experimental tool kit" work... trying to understand some complex (charge build up?) behavior in the intense FE beam.

As it is, I have to manual move the stage when acquiring counts and absorbed beam current, to hit 'unzipped' areas every second or so...seems like PfE should have this option (even if vulcan power fist salut required).

Hi John,
I understand. But for a specialized measurement you could use Gopon's Lab View interface to my instrument API, couldn't you?   After all, that is exactly what the Remote API is for!

I'd rather spend my time adding features that everyone can use.

Edit by John: this feature is now available as described here:

https://smf.probesoftware.com/index.php?topic=42.msg8434#msg8434
The only stupid question is the one not asked!

John Donovan

Quote from: John Donovan on April 03, 2015, 06:54:21 PM
Quote from: JohnF on April 03, 2015, 06:17:02 PMWorking with FE probe means a much more intense beam, so there is (or should be) a certain amount of experimentation. Certainly TDI is one useful tool. Another useful tool would be the ability to jog the stage (or continuously move it) while counting either as a standard or an unknown (clearly on a homogeneous material). In PfE there is a clear ability to do this with wavescans. However, I do not see it for unknown or standard acquisitions. Is it there somewhere, where I just don't see it? Or it not there, it would be a useful addition to the PfE toolkit.

Hi John,
Yes, the stage stepping option for wavescans as seen here:



...was designed for sulfur peak shift measurements for determining chemical oxidation state.  The problem is that if one leaves the beam too long on an alkali glass, the trace sulfur will begin to oxidize, compromising the peak shift characterization...

But I do understand your point, so try the Alternating on/off Peak method.  This tracks the net intensity over time.

And if the sample really is homogeneous, why not just defocus the beam?
john

Someone recently asked about moving the stage during a sample acquisition and we found that the above screen shot is slightly out of date.  Here is a more recent screen shot which allows the stage to be incremented during unknown acquisitions:

John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"