Digitize Image - how to set up a lot of BSE images?

Started by AndrewLocock, December 20, 2016, 09:32:02 AM

Previous topic - Next topic

AndrewLocock

Hello,
I have a mount of more than 250 grains for which I would like individual BSE images, but not point analyses.
How can I use Digitize Image in Probe-for-EPMA to set up a lot of BSE images (at about the same magnification),
and run them automatically (as a batch)?

Thanks,
Andrew

John Donovan

#1
Quote from: AndrewLocock on December 20, 2016, 09:32:02 AM
Hello,
I have a mount of more than 250 grains for which I would like individual BSE images, but not point analyses.
How can I use Digitize Image in Probe-for-EPMA to set up a lot of BSE images (at about the same magnification),
and run them automatically (as a batch)?

Thanks,
Andrew

Hi Andrew,
There are probably several ways to do this, but one method that comes to mind is to utilize the feature normally used to acquire mosaic images, and that is to digitize the image centers in the Stage app and then use the Confirm All Positions and Acquire Images With Confirm checkboxes as seen here: