Ben Buse

Hi John,

Any chance you could remove the popup window 'bad negative zz' and just log the error message. The problem is it opens the window consecutively many times.

When processing the data, do you do anything different with bad negative zz values. Once I've clicked the message box 20-30x the data often seems ok.


Thanks

Ben

John Donovan

Quote from: Ben Buse on August 14, 2019, 02:37:46 AM
Hi John,

Any chance you could remove the popup window 'bad negative zz' and just log the error message. The problem is it opens the window consecutively many times.

When processing the data, do you do anything different with bad negative zz values. Once I've clicked the message box 20-30x the data often seems ok.


Thanks

Ben

Hi Ben,
I don't do anything with the negative ZZ value, but the matrix correction physics calculations cannot proceed (usually). 

Can you send me the MDB file which contains the problem data points?
john
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Ben Buse

Hi John,

Thanks for explaining.

I'll email you.

Ben

John Donovan

Quote from: Ben Buse on August 14, 2019, 02:37:46 AM
Hi John,

Any chance you could remove the popup window 'bad negative zz' and just log the error message. The problem is it opens the window consecutively many times.

When processing the data, do you do anything different with bad negative zz values. Once I've clicked the message box 20-30x the data often seems ok.


Thanks

Ben

Hi Ben,
I modified the matrix correction error messages to just log the error to the log window when it encounters negative values for certain mathematical operations.  You can update to Probe for EPMA v. 12.7.1 whenever you are ready.

Let me know if this works better for you.
john
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Philipp Poeml

Hi, when switching through many of the PfE windows using the TAB key the order in which the fields are selected seems totally random. Is it possible to bring this in order to press TAB and really move to the next field?

John Donovan

Hi Philipp,
It is possible, and you may find some windows are better organized than others.  To be honest, it has not been a priority.  Which windows specifically are you looking at?

Also, we've tended to only allow tabbing for the text input controls. How do you feel about that?
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

Philipp Poeml

Hi John,

it's various windows... For example in the elements/cations, when I edit an element, or when I use the "edit mac table".
I can see that it is not a priority... There is more important stuff to do. But maybe, when changing some window, the tab order could be checked.

I use TAB and ENTER quite a lot... I am not a big fan of clicking around with the mouse. So I use TAB also to move from "cancel" to "ok" and hit enter.

Nice would be also some keyboard shortcuts... In calczaf you can open the X-ray menu using alt-x, but then there are no furhter keys defined for the submenu.

Cheers
Philipp

glennpoirier

Hi John and Philipp,
I especially agree with Philipp's request for some shortcut keys! One I'd really appreciate would be the Single Points menu on the Digitize positions window.
I'd then be able to assign that key combination to a USB foot pedal and store points without taking my eyes off the JEOL SEM screens. It's all about productivity! ;)

Cheers

Glenn

John Donovan

Quote from: glennpoirier on September 17, 2019, 09:39:52 AM
Hi John and Philipp,
I especially agree with Philipp's request for some shortcut keys! One I'd really appreciate would be the Single Points menu on the Digitize positions window.
I'd then be able to assign that key combination to a USB foot pedal and store points without taking my eyes off the JEOL SEM screens. It's all about productivity! ;)

Cheers

Glenn

Hi Glenn,
I could add an <alt> S key shortcut for the Single Points button. 
john
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

glennpoirier

That would be perfect!
Thanks
Glenn

John Donovan

Quote from: glennpoirier on September 17, 2019, 10:51:45 AM
That would be perfect!
Thanks
Glenn

Or maybe I'll make the Single Points button an <alt> P and the Shotgun button an <alt> S?
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"

glennpoirier


BenjaminWade

Hi John
My wish would be to have the list of standards in the MAN fit window sorted by standard number. I am not too sure what is governing the order they appear at the moment, it doesnt appear to be mean Z.

Cheers

Karsten Goemann

I second the suggestions for keyboard shortcuts and tab key sequencing. Like Philipp working with the keyboard is much quicker for me than constantly having to put one hand back on the mouse and point that to the next field.

One of my favourite candidates to have the tab key progress through the fields in order (left->right, top->bottom) would be the Element/Cation Properties window, especially the WDS Spectrometer Parameters section.

Cheers, Karsten

John Donovan

Quote from: Karsten Goemann on September 17, 2019, 07:03:55 PM
I second the suggestions for keyboard shortcuts and tab key sequencing. Like Philipp working with the keyboard is much quicker for me than constantly having to put one hand back on the mouse and point that to the next field.

One of my favourite candidates to have the tab key progress through the fields in order (left->right, top->bottom) would be the Element/Cation Properties window, especially the WDS Spectrometer Parameters section.

Cheers, Karsten

We'll start working on that. Also we'll take a look at the MAN standards list order as Ben Wade mentions.
John J. Donovan, Pres. 
(541) 343-3400

"Not Absolutely Certain, Yet Reliable"